Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kraton D1192 ETF - SBS - Kraton Polymers

Material Data Center offers the following functions for Kraton D1192 ETF:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kraton D datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Kraton D1192 E is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass.
Kraton D1192 ETF - supplied as fluffy crumbs dusted with talc.
加工/物理特性价值单位Test Standard
ISO数据
熔融指数, MFI 1 g/10min ISO 1133
温度 200 °C -
负载 5 kg -
机械性能价值单位Test Standard
ISO数据
拉伸强度 33 MPa ISO 37
断裂伸长率 1000 % ISO 37
ASTM数据
邵氏硬度A 70 - ASTM D 2240
Other Standards[S]
300%应变时的应力 14.4 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
其它性能价值单位Test Standard
Bulk density 400 kg/m³ -
Other Standards[S]
密度 940 kg/m³ ISO 2781
S: These properties are reported by the producer according standards that are different to our defaults.
典型数据
加工方法
表面涂层
特殊性能
透明.
特征
共聚物
耐化学试剂
抗氧化性
地区供应
北美, 欧洲, 亚太, 中东/非洲
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.